#49002
Grmps
Participant
  • Bronze
  • Posts: 2
  • Comments: 20
  • Overall: 22

They are TGIC Polyester, they should shoot just fine, I have too many projects going. https://www.eastwood.com/eastwood-extreme-chrome-bonded-powder.html

Eastwood Extreme Chrome Bonded Powder
Item #15999 Extreme Chrome Bonded Powder

SPECIFICATIONS
Color: Chrome
Gloss Level: Gloss
Cure Temperature: 400 Degrees
Cure Time: 20 Minutes after flowout
Powder Type: High-Tech, Bonded Polyester-TGIC
Finish: Smooth
Coverage: 1/2 lb. of powder is approximately 10-20 sq. ft.

They recommend a clear coat for long-term durability, I think it makes the chrome duller.

I used the ASBBDT (Air Soft BB Dry Tumble method)

cover the bottom of a #5 container with ASBB’s, toss in 1 tsp powder and a handful of bullets.

close lid and swirl for 15 – 30 seconds. Dump into a colander with holes large enough for the BB’s to fall through and shake off all the excess powder. Chrome is a little more finicky so I grab the pc’d bullets with a tweezer, make sure all excess powder is of by tapping tweezer on side of bowl then stand up in baking basket, Normally I just dump the bullets into the baking basket and go 12 min@ 400° in a preheated oven

[img]https://i.imgur.com/aEnopDb.jpg[/img]